< 3 %lattice mismatch, fluorite buffer
vs ≈ 25 % for LSMO
A buffer from the same family
On CGO and YSZ, HZO grows with a dominant (200) orientation through a fluorite–fluorite interface. On LSMO it grows (111)-oriented with several in-plane variants, by domain-matching epitaxy. Synchrotron reciprocal space maps show the buffers rotated 45° on Nb:SrTiO3 and orthorhombic and monoclinic HZO coexisting, so the buffer decides which polymorph orientations appear.
> 3×piezoresponse with an
oxygen-conducting buffer
Stronger and conventional electromechanics
SS-PFM and cKPFM show two stable polarization states and a piezoresponse more than three times larger than without the ionic buffer. Calibrated PFM gives positive electrostriction coefficients, as in BaTiO3 or PZT, and a large reversible component of the response under field.
≈ 10–11 μC cm−2ferroelectric polarization in HZO,
HZO/CGO stack
Polarization without PUND
Field-driven vacancy redistribution makes the electronic conductivity history-dependent, so PUND subtraction fails in these stacks. About 15 μC cm−2 is taken from the clean switching peak under negative bias, and a two-layer electrostatic model assigns 10–11 μC cm−2 to HZO. CGO-buffered devices leak far less than LSMO-buffered ones, with trap-limited, injection-limited and space-charge-limited regimes in turn.
|V| > 0.2 Vonset of a slow, low-frequency
impedance arc
An ionic signature in the switching
At zero bias the impedance is a single bulk arc (≈ 2 GΩ, ≈ 5 pF). Under bias a space-charge element and then a diffusion-related element appear. Switching is strong near 1 kHz and fades at 10 kHz, pointing to slow ionic motion coupled to polarization. The buffer acts both as a dielectric that blocks direct electronic transport and as a channel for vacancies into and out of HZO.
±200 kV mm−1in situ scanning nano-XRD,
88 nm beam
The polar phase holds, locally rearranged
No monoclinic or tetragonal signature appears during field cycling. Average strain, tilt and peak width change little, while their spatial spread changes more. HR-TEM after cycling shows modulated oxygen order in HZO and double-fluorite nanodomains in the CGO, consistent with vacancy exchange without a global phase transition.