2.38 × 10−14m2 V−2, CGO/ESB multilayer;
≈ 103 × best relaxors
A thousand times the best relaxors
The multilayers are grown on NdGaO3 cantilevers with planar gold electrodes on top. A sinusoidal field bends the cantilever, and the free-end displacement is read by laser interferometry at twice the drive frequency, the signature of a quadratic response. Simple oxides sit below 10−19 m2 V−2.
≈ 1 %in-plane mismatch, CGO rotated
45° on NdGaO3
Coherent, atomically sharp interfaces
X-ray diffraction and reciprocal space maps show phase-pure, epitaxial films with smooth interfaces. Electron microscopy finds coherent CGO/ESB interfaces without dislocations: the two lattices are forced to share one in-plane spacing, so each interface stores a lattice discontinuity as elastic strain.
M ↑ as Λ ↓more interfaces per
film thickness
The interfaces do the work
Shrinking the CGO/ESB period packs more interfaces into the same film and raises the coefficient, until the layers become too thin to stay chemically distinct. Atomistic calculations trace the enhancement to coherent strain imparted by the interfacial lattice discontinuity.
p → εelectric dipoles carry
a mechanical footprint
Defect dipoles that steer strain
In the simulations, dopants and oxygen vacancies create local electric dipoles through off-centre ion displacements. Without a field they point every way. Under a field they align and grow, and the resulting energy change is dominated by elastic strain. Thinner periods make the dipoles easier to steer. Because each local distortion keeps its axis when the field reverses, the strain follows the square of the field.
17.4 kV cm−1cycled at 1, 50 and 200 Hz
Stable under cycling
Under a constant-amplitude sinusoidal field the response shows no degradation over repeated cycles at 1, 50 and 200 Hz. The coefficient is largest at low frequency and decreases as the drive gets faster.